Steel grade
Steel grade |
Chemical composition, % |
Notes |
C |
Si |
Mn |
P |
S |
Soft magnetic iron plates TAD |
≤0.03 |
≤0.04 |
≤0.50 |
≤0.030 |
≤0.030 |
|
Mechanical properties
Steel grade |
Application |
Hardness |
Tensile strength,
N/mm2 |
Elongation, %
(1.0 mm thick) |
Bending R=0.2 90° |
For drawing |
For punching or bending |
HV |
HRBS |
Soft magnetic iron plates TAD |
○ |
- |
≤110 |
≤62 |
260≤ |
39≤ |
No fissures on outer face of test piece |
- |
○ |
100 - 140 |
56 - 75 |
270 - 400 |
- |
Magnetic properties
[ JIS C 2504:2000 ]
Type and symbol |
Coercivity, A/m |
Magnetic flux density, T |
Magnetic field strength, A/m |
100 |
200 |
300 |
500 |
1000 |
4000 |
SUY-0 |
≤60 |
0.90≤ |
1.15≤ |
1.25≤ |
1.35≤ |
1.45≤ |
1.60≤ |
SUY-1 |
≤80 |
0.60≤ |
1.10≤ |
1.20≤ |
1.30≤ |
1.45≤ |
1.60≤ |
SUY-2 |
≤120 |
- |
- |
1.15≤ |
1.30≤ |
1.45≤ |
1.60≤ |
SUY-3 |
≤240 |
- |
- |
1.15≤ |
1.30≤ |
1.45≤ |
1.60≤ |
[ JIS C 2504:1990 ]
Type and symbol |
Coercivity, A/m |
Magnetic flux density, T |
B1 |
B2 |
B3 |
B5 |
B25 |
SUYP0 |
≤63.2 |
0.80≤ |
1.10≤ |
1.25≤ |
1.35≤ |
1.55≤ |
SUYP1 |
≤79.1 |
0.50≤ |
1.00≤ |
1.20≤ |
1.35≤ |
1.55≤ |
SUYP2 |
≤103 |
0.20≤ |
0.75≤ |
1.10≤ |
1.30≤ |
1.55≤ |
SUYP3 |
≤142 |
0.10≤ |
0.40≤ |
0.08≤ |
1.10≤ |
1.50≤ |